Der Blätterkatalog benötigt Javascript.
Bitte aktivieren Sie Javascript in Ihren Browser-Einstellungen.
The Blätterkatalog requires Javascript.
Please activate Javascript in your browser settings.
7 ACCREDITED TEST LABORATORY Plastics Plastics and rubber are tested for their hardness in a climate controlled room at a constant temperature and humidity To determine the hardness on elastomers or thermoplastic elastomers we offer standardized tests using the testing method Shore A For very small specimens we use the standardised IRHD microhardness test method M In addition we are even able to test components with a minimum material thickness of 0 5 mm by using the Micro Shore Amethod Standardised hardness testing for plastics e g according to • DIN ISO 7619-1 • DIN EN ISO 868 • DIN ISO 48